Show simple item record

dc.contributor.authorWakchaure, Kiran
dc.contributor.authorChaudhari, Rakesh
dc.contributor.authorThakur, Ajaykumar
dc.contributor.authorFuse, Kishan
dc.contributor.authorLópez de Lacalle Marcaide, Luis Norberto
dc.contributor.authorVora, Jay
dc.date.accessioned2023-08-07T12:31:59Z
dc.date.available2023-08-07T12:31:59Z
dc.date.issued2023-06-22
dc.identifier.citationMetals 13(7) : (2023) // Article ID 1159es_ES
dc.identifier.issn2075-4701
dc.identifier.urihttp://hdl.handle.net/10810/62125
dc.description.abstractSubmerged friction stir welding (SFSW) is a new modification of friction stir welding. In this paper, 6 mm thick 6061Al-T6 alloy plates were welded using the friction stir technique under normal air and submerged water conditions at 108 mm/min welding speeds and a rotational rate of 900 rpm. The cooling water temperature in SFSW varied at 0 °C, 35 °C, and 80 °C to clarify the effect of water temperature. The characteristic hourglass-shaped stir zone was observed in the macrostructure of all the samples. All the samples exhibited defect-free joints. The results revealed that the finer grain size of 2.43 μm was at 0 °C. The macrostructure of SFSW joints separated into the shoulder-driven zone and pin-driven zone due to the low-temperature difference between the environment and water media and the high heat absorption capacity of the water, which caused a more substantial cooling rate during water-submerged welded joints. The microhardness distribution of all the joints showed typical “W” shape characteristics. The microhardness for all submerged samples was higher than in normal air conditions due to the higher thermal cycling effect in submerged conditions. Improved dynamic recrystallization in the joint welded at 80 °C resulted in the highest tensile strength (~249 MPa) and microhardness (~95 HV).es_ES
dc.language.isoenges_ES
dc.publisherMDPIes_ES
dc.rightsinfo:eu-repo/semantics/openAccesses_ES
dc.rights.urihttp://creativecommons.org/licenses/by/4.0/
dc.subjectfrictiones_ES
dc.subjectgreenes_ES
dc.subjectmicrostructurees_ES
dc.subjectsubmergedes_ES
dc.subjectweldinges_ES
dc.titleThe Effect of Cooling Temperature on Microstructure and Mechanical Properties of Al 6061-T6 Aluminum Alloy during Submerged Friction Stir Weldinges_ES
dc.typeinfo:eu-repo/semantics/articlees_ES
dc.date.updated2023-07-28T12:21:37Z
dc.rights.holder© 2023 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/ 4.0/).es_ES
dc.relation.publisherversionhttps://www.mdpi.com/2075-4701/13/7/1159es_ES
dc.identifier.doi10.3390/met13071159
dc.departamentoesIngeniería mecánica
dc.departamentoeuIngeniaritza mekanikoa


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record

© 2023 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/ 4.0/).
Except where otherwise noted, this item's license is described as © 2023 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/ 4.0/).